Creep of Nextel™610 Fiber at 1100°C in Air and in Steam
Document Type
Article
Publication Date
3-2013
Abstract
Excerpt: Creep of Nextel™610 fibers was investigated at 1100°C and 100–500 MPa in air and in steam. The effect of loading rate on fiber tensile strength was also explored. The presence of steam accelerated creep and reduced fiber lifetimes.
Source Publication
International Journal of Applied Ceramic Technology (ISSN 1546-542X | eISSN 1744-7402)
Recommended Citation
Armani, C.J., Ruggles-Wrenn, M.B., Fair, G.E. and Hay, R.S. (2013), Creep of Nextel™ 610 Fiber at 1100°C in Air and in Steam†. Int. J. Appl. Ceram. Technol., 10: 276-284. https://doi.org/10.1111/j.1744-7402.2012.02831.x
Comments
© 2013 The American Ceramic Society
The full article is available from Wiley via subscription or purchase, using the DOI link below.